27612866

9783846534717

Stress Corrosion Cracking of X-70 steel in carbonates, solutions: Stress Corrosion Cracking of X-70 Microalloyed steel in carbonates, chlorides and sulfates solutions

Stress Corrosion Cracking of X-70 steel in  carbonates, solutions: Stress Corrosion Cracking of  X-70 Microalloyed steel in  carbonates, chlorides and sulfates solutions
$129.57
$3.95 Shipping
  • Condition: Good
  • Provider: Bonita Contact
  • Provider Rating:
    0%
  • Ships From: Multiple Locations
  • Shipping: Standard
  • Comments: Access codes and supplements are not guaranteed with used items. May be an ex-library book.

seal  

Ask the provider about this item.

Most renters respond to questions in 48 hours or less.
The response will be emailed to you.
Cancel
  • ISBN-13: 9783846534717
  • ISBN: 3846534714
  • Publication Date: 2011
  • Publisher: LAP LAMBERT Academic Publishing

AUTHOR

Bernardo Campillo, Alvaro Torres, Sergio Serna

SUMMARY

Bernardo Campillo is the author of 'Stress Corrosion Cracking of X-70 steel in carbonates, solutions: Stress Corrosion Cracking of X-70 Microalloyed steel in carbonates, chlorides and sulfates solutions', published 2011 under ISBN 9783846534717 and ISBN 3846534714.

[read more]

Questions about purchases?

You can find lots of answers to common customer questions in our FAQs

View a detailed breakdown of our shipping prices

Learn about our return policy

Still need help? Feel free to contact us

View college textbooks by subject
and top textbooks for college

The ValoreBooks Guarantee

The ValoreBooks Guarantee

With our dedicated customer support team, you can rest easy knowing that we're doing everything we can to save you time, money, and stress.